Hi gents,

I am here with an interesting query (May be only to me). Could someone help me?

1. Can ICCP prevent susceptible materials from ESCC?
2. Can Galvanic anodes prevent susceptible materials from ESCC?
3. NACE SP0198 specifies Al-foil as a prevention method for ESCC for SS. My question is, whether the physical barrier effect or galvanic effect is helping in preventing ESCC for SS?

Please share your views.

CocoE
 