Are there any proper techniques or tricks to preventing pipe from bowing on a lateral weld? Connecting 16" pipe to 14" branches steel piping. Any help is appreciated. Thanks Jim.
 
Can you provide a sketch of what you are talking about? To prevent or fix bowing, we always either build negative camber into the jig or use a torch to heat certain areas after welding.
 
Assuming that you may not be able to support the run pipe during welding, weld with the o'let branch in the 3:00 position using small diameter electrodes.
 
Jim...

What are the materials being welded and what is the schedule of the stainless piping ?

If the piping is thinner than 10S schedule, it can be a horror show to weld.

How about a sketch ???

MJCronin
Sr. Process Engineer
Venture Engineering & Construction
 