Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations The Obturator on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Pressure vessel dish design

Status
Not open for further replies.

ak.myakala

Mechanical
Mar 30, 2017
1
How to make a template of crown and patel type hemispherical dish or how to fabricate it? how to calculate crown radius and templete for patel?.....is there any book to refer for same
 
Replies continue below

Recommended for you

Our company doesn't do any head forming, but we have bought a number of crown/petal hemispherical heads from vendors.

I would imagine a lot of the design is based on material availability and forming capacity at the shops. A couple of ideas...
[ul]
[li]Crown diameter is probably limited by two factors, available plate width and forming capacity. Depending on your material (CS vs. SS), typically 8ft or 10ft wide plates are available, so one limit on maximum crown diameter is likely the largest diameter that can be formed from the available plate width. Another limit on maximum diameter is likely the capacity of the machinery being used by the supplier.[/li]
[li]For petal design, it's probably a similar decision basis. You know the circumference of your vessel, and you know the available plate widths. So one way of selecting the number of petals could be: Number of petals = (Circumference) / (Available plate width)[/li]
[/ul]
 
A little late, nonetheless check this site as there is a fair amount of summary into forming various head types:
Baker Tankhead manufacturers standard and A.S.M.E. tank heads, hot-formed heads, cones, manways and rolled shells in Fort Worth Texas at http:
 