Hello everyone!
I have a nozzle which is welded through shell and jacket plates. We are having a trouble making a fillet weld on the outside surface of a shell, because there is practically no access.
Is there any type of weld that allows making only full penetration groove weld without making a fillet weld on the backside?
I have a nozzle which is welded through shell and jacket plates. We are having a trouble making a fillet weld on the outside surface of a shell, because there is practically no access.
Is there any type of weld that allows making only full penetration groove weld without making a fillet weld on the backside?