Can anyone please help / guide me to an international standard for the pressure temperature ratings of Titanium valves.
 
Replies continue below

Recommended for you

Mike, many thanks for the reply. No manufacturer seems to publish this info.
 
Refer to the appendix in ASME B16.34. It provides a method for calculating pressure-temperature ratings.
 