mrcadman2u
Aerospace
I am designing a part that is Titanium 6-4 and a shaft made of MP35N to be press fit into Ti part. The shaft is .625 and needs to be symmetrical in Ti part that is about 1.5 in long supports the shaft. The shaft is approx 7 inches long so needs to be pressed about 3.5 inches. The question that is debatable is what type of fit do I need to produce the desired result. Currently the hole is nominal .75 +.0005 -.0000 and the shaft is .75 +.0005 -.0000.
More info if you need it.
Thanks in advance.
Jerry L. Eden
Mechanical Designer
More info if you need it.
Thanks in advance.
Jerry L. Eden
Mechanical Designer