In our manufacturing process, we press a .1212/.1215 OD 303 SS insert into a .1207/.1210 ID SS body to a depth of .060 inches. The problem we are having is leaking between the insert and body in excess of 0.2 SCCM. We realize that similar metals should not be used in this assembly, unfortunately this being a medical application changing material is slow and difficult.
We have tried press to a lessor depth and the leak has dropped. Next, we're machining a counter-bore hole for alignment before the press fit section.
Any ideas for a permanent fix?