Pre-heating frequently is used to avoid losing all the heat in the carburizing furnace (which is > 900 degrees C) when you open the door and put in a large mass of parts and fixturing that is at room temperature.
How big is this part (dimensions and mass)? Are there thick-to-thin transitions? Another reason to pre-heat is to achieve temperature uniformity through the different cross-sections.