preheat requirements for A992 2

Status
Not open for further replies.

Prestressed Guy

Structural
May 11, 2007
390
Can someone share the Dd.1 preheat table 4.3 that lists the preheat requirements for heavy A992 sections?
 
Replies continue below

Recommended for you

Here's an excerpt of AWS D1.1-15 Table 3.3 (I assume this is what you were asking for):

Screenshot_2022-07-14_131556_tltu5g.jpg
 
Yep, that is it. I only have a very old AWS given that I do exclusively precast/prestressed concrete and that mostly uses small welds in single pass fillets and flare bevel so have not invested in a newer AWS but need to do some welding on 2" A992. I was assuming that it would be 150ºF like the other grade 50 steel but wanted to make sure.
 
Ok, time to split hairs.
Given an A992 beam with a 2.48" flange (W27x368) what preheat temperature should be called out?

Per table 3.3
1½" to 2½" inc. preheat to 150ºF
over 2½" preheat to 225ºF

So, by the book preheat to 150ºF. BUT... if it was 0.03" thicker, it would need to preheat to 225ºF. That is a mighty big change in temperature for a very little difference in thickness.

What say you, 150º, 225º or something in between?
 