A plate was welded to a column by E6010(ASME standard of electrode) as root pass and E6013 (ASME standard of electrode)as filling passes. All materials are st37 and the thickness of base plate is 25 mm and it should be preheated about 70 C in conformance with ASME, but it wasn't preheated.
How can I test the column to determine whether we can use it in the structure or not?
I should add that the results of all N.D.T.s including U.T.,M.T.,V.T. are accepted but I can't reffer to them to judge about the soundness of the weld in this case, can I?
And what is the solution to overcome such a problem after welding?
I would appreciate any suggestion,
GHAN.
A plate was welded to a column by E6010(ASME standard of electrode) as root pass and E6013 (ASME standard of electrode)as filling passes. All materials are st37 and the thickness of base plate is 25 mm and it should be preheated about 70 C in conformance with ASME, but it wasn't preheated.
How can I test the column to determine whether we can use it in the structure or not?
I should add that the results of all N.D.T.s including U.T.,M.T.,V.T. are accepted but I can't reffer to them to judge about the soundness of the weld in this case, can I?
And what is the solution to overcome such a problem after welding?