Hi
i am a little bit confused about tolerances given for induction hardened and hard chrome plated linear shaft
(see attachment)
let's analyze diameter 4: for ISO h7 tolerance, default circularity at level 0.005 - ok for me
cylindricity (parallelism) at level 0.01 - ok for me
but straightness - 0.3/1000 = 0,0003 ????
straightness must be usually lower than circularity - but is it ever possible to machine such a good way?....
or maybe I miscalculated something here?
I reviewed also Bosch Rexroth specifications, they are using similar descriptions and values
but why not to use runout as it is a mix of circularity of straightness?
M
i am a little bit confused about tolerances given for induction hardened and hard chrome plated linear shaft
(see attachment)
let's analyze diameter 4: for ISO h7 tolerance, default circularity at level 0.005 - ok for me
cylindricity (parallelism) at level 0.01 - ok for me
but straightness - 0.3/1000 = 0,0003 ????
straightness must be usually lower than circularity - but is it ever possible to machine such a good way?....
or maybe I miscalculated something here?
I reviewed also Bosch Rexroth specifications, they are using similar descriptions and values
but why not to use runout as it is a mix of circularity of straightness?
M