WHAT IS A GOOD SLUMP REQUIREMENT FOR PRECAST CONCRETE PILE?
WHAT IS A GOO SIDE CLEARANCE FOR POURING?
IS ROTATION OK FOR AURGER PILES NOT GOOD DURING PUMPING?
 
Replies continue below

Recommended for you

Slump:
Depends on required strength and the batch mix (w/ or w/o admixtures)

Concrete Cover (manufactured under plant control conditions):
Exposed to Earth => #6 bar (.75" diam.) to #11 bar (1.41" diam.) requires 1.5" cover
#5 bar (.625" diam) and smaller requires 1.25" cover

Auger Piles: not clear as to what you are asking.
 
it is mix with 4000 psi w/ admixtures
cover 2 1/2" w/ #6 bars 50 ton Capacity
 