Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Practical Implications of Impact Testing 2

AgsMyDude

Mechanical
Joined
Jul 28, 2021
Messages
35
Location
US
I've always specified materials that don't require impact testing but I don't have a great understanding of what the practical implications would be if the testing is required (for instance if A53B is specified for use below its curve in Fig 323.2.2-1 of B31.3).

In a general sense...

Does it mean the fabricator needs to add some extra length that can be removed and sent off for testing? Or does the fabricator have certifications for materials (say A53B) that have already been tested that they can hand to you? If the former, what happens if the toughness comes back too low at the design minimum temperature given the pipe is already being fabricated? It seems like it would "too late" at that point and a re-design would be required.

How do we not already know the toughness of standard materials of construction as a function of temperature?

How would a field weld be tested?

Thanks in advance
 
Last edited:
When you buy the material it should be certified by the supplier to meet the requirements for impact strength as well as all its other rated properties.

I think that the toughness of standard materials of construction is already known as a function of temperature. You just need to find the right references.

I don't know how you'd handle weld impact strength. I would think that the welding process could add a lot of variation. You could always design using the fully annealed strength and add a safety factor.
 
Thanks for the response.

I read that toughness testing is typically required as a part of material specs but additional testing per Table 323.2.2-1 is required to use the material below its line in Fig 323.2.2-1. What happens in this instance? Are we just *hoping* the material comes back tougher (I am not sure why it would)?

Edit: I do see Table 323.3.5-1 with the minimum toughness energies but still looking for clarification on the other points.
 
Last edited:
I've always specified materials that don't require impact testing but I don't have a great understanding of what the practical implications would be if the testing is required (for instance if A53B is specified for use below its curve in Fig 323.2.2-1 of B31.3).

In a general sense...

Does it mean the fabricator needs to add some extra length that can be removed and sent off for testing? Or does the fabricator have certifications for materials (say A53B) that have already been tested that they can hand to you? If the former, what happens if the toughness comes back too low at the design minimum temperature given the pipe is already being fabricated? It seems like it would "too late" at that point and a re-design would be required.

How do we not already know the toughness of standard materials of construction as a function of temperature?

How would a field weld be tested?

Thanks in advance
The answer is simple. You will ask for impact tested materials at the time of order. Impact testing is determined by the process/mechanical determined MDMT. It's a design parameter.
Once you know the MDMT, you can use Fig. 323.2.2-1 to determine is an impact test will be required for the base material and also by using Table 323.2.2 for both base metal and weld metal.
There will be no practical implications for both base and weld metal if you know the impact test requirements prior to starting your material procurement and fabrication.
I believe you know the importance of impact test requirement for low temperature service. Many pressure vessels have encountered brittle facture during hydrotesting because they had high MDMT but didn't consider the room temperature for a hydrotest.
 
Thanks for the response.

I read that toughness testing is typically required as a part of material specs but additional testing per Table 323.2.2-1 is required to use the material below its line in Fig 323.2.2-1. What happens in this instance? Are we just *hoping* the material comes back tougher (I am not sure why it would)?

Edit: I do see Table 323.3.5-1 with the minimum toughness energies but still looking for clarification on the other points.
Sorry, I don't have access to Table or Figure 323.2.2-1, so I can't comment.
 
The answer is simple. You will ask for impact tested materials at the time of order. Impact testing is determined by the process/mechanical determined MDMT. It's a design parameter.
Once you know the MDMT, you can use Fig. 323.2.2-1 to determine is an impact test will be required for the base material and also by using Table 323.2.2 for both base metal and weld metal.
There will be no practical implications for both base and weld metal if you know the impact test requirements prior to starting your material procurement and fabrication.
I believe you know the importance of impact test requirement for low temperature service. Many pressure vessels have encountered brittle facture during hydrotesting because they had high MDMT but didn't consider the room temperature for a hydrotest.
Thanks GD2, I understand MDMT selection and the purpose of Fig. 323.2.2-1. What I'm struggling with is the fundamentals of specifying a material that requires impact testing.

Why would we expect an impact-tested material to perform any better than the same material that has not been impact tested? Does the request for impact testing actually change the material spec? How can we guarantee it will pass the impact test after you have specified it?
 
Try a Google search on “Review of the effects of steel composition and heat treatment on Charpy energy toughness”, or try a variant prompt in your bot of choice. It’s not really a question of ‘expectation’ rather one of ‘verification’
 
Thanks Steve, are you implying that an impact toughness spec typically results in a heat treatment of the base metal to achieve the desired toughness value?

I think this may be the gap in my understanding. Heat treatment is only mentioned sparingly in paragraphs relating to low temperature service.
 
Thanks GD2, I understand MDMT selection and the purpose of Fig. 323.2.2-1. What I'm struggling with is the fundamentals of specifying a material that requires impact testing.

Why would we expect an impact-tested material to perform any better than the same material that has not been impact tested? Does the request for impact testing actually change the material spec? How can we guarantee it will pass the impact test after you have specified it?
Ok. Let me try my best to explain this. Doing an impact test doesn't change the material property, rather it provides the confidence that the material will have enough toughness at the tested temperature (typically this will be the Test MDMT). This is built on the premise that some CS and low alloy steels loses ductility at reduced temperature.
ASME had developed the UCS -66 curves in ASME Sec VIII Div 1 (later taken by the Piping Code ASME B31.3) based on the material toughness, thickness and stress levels to determine safe operating temperatures. These curves are essentially a simplified representation of fracture mechanics principles, providing a practical way to assess the need for impact testing.
You must be aware that not all materials are factory impact tested during it's manufacturing process. Example of factory impact tested materials are A333 Gr. 6 and SA-352 LF2. The vast majority of materials are not. Impact testing is expensive and becomes a cost adder to the owner/fabricator.
ASME have, therefore, made it easier for the designer/fabricator to build pressure vessels/pressure piping without the need to do an impact test, where not required.
Rather, it has provided the criteria for impact testing through Fig. 323.2.2A and Fig. 323.2.2B.
 
Thanks for sticking with me on this. Would it be safe to say that most materials not already impact tested as part of their manufacturing process are rarely used below their line on Fig. 323.2.2-1?

Say I intend to use A333 Gr6 (min temperature of -50F according to B31.3) at a slightly lower temperature (-55F). I assume when we specify the material, we would just indicate to the fabricator the requisite toughness at MDMT (-55F in our case) and they may change the heat treat to get it to pass at that temperature? If no change to heat treat is required to for acceptability at -55F, then why the limit of -50F?
 
Would it be safe to say that most materials not already impact tested as part of their manufacturing process are rarely used below their line on Fig. 323.2.2-1?
Yes, but it is possible. To your example of A333 Grade 6 at -55F, it is simply a matter of specifying additional testing and ensuring you have the material to test. The manufacturer may be able to just lower their test temperature, but only if you are buying in large quantity. More typically you'll buy the pipe from a stockist and have to buy a little extra to do the supplementary testing. You could review the standard test results at -50F and pick pipe from a heat that has the best chance of passing at the lower temperature.

If no change to heat treat is required to for acceptability at -55F, then why the limit of -50F?
Because it's relatively "easy" to achieve -50F consistently with the right steel chemistry, process controls, and heat treatment. That is also a common MDMT required by operators. Lower temperatures mean more chance of a heat failing to meet the standard and not being able to mark it as such, which is a costly failure for a manufacturer.
 
Thanks, it is clicking for me now.

And so were I inclined to use a material "below it's line" (whether it is typically impact tested or not), I'd probably need to request historical impact test data from manufacturers and decide for myself whether I think it is safe to use/will pass the tests required by B31.3.
 
Thanks, it is clicking for me now.

And so were I inclined to use a material "below it's line" (whether it is typically impact tested or not), I'd probably need to request historical impact test data from manufacturers and decide for myself whether I think it is safe to use/will pass the tests required by B31.3.
Why historical? You know with modern steel mills, steel manufacturing process have changed, and also it's quality. You need to make sure that you test the material you are going to install. It goes by Heat No.
You might get away without impact testing, if you follow the rules of Para 323.2.2. It provides few criteria to lower the MDMT. Try to apply these, before you order the impact test.
 
Historical in the sense of impact tests or toughness values that were generated recently but prior to execution of my project.

The materials of construction are often selected well before a fabricator is engaged or properties such as stress ratio are defined.
 
Aside from low temp toughness tests and grain quality, all carbon steel / low alloy carbon steel grades used in subzero temp applications are silicon killed steels as far as I know. What about this batch of A53 pipe ?
 
Aside from low temp toughness tests and grain quality, all carbon steel / low alloy carbon steel grades used in subzero temp applications are silicon killed steels as far as I know. What about this batch of A53 pipe ?
I don't think it is mandatory to have killed steel for low temp service, but preferred as killed steel improves the toughness.
 
Historical in the sense of impact tests or toughness values that were generated recently but prior to execution of my project.

The materials of construction are often selected well before a fabricator is engaged or properties such as stress ratio are defined.
I don't think you got it right. When you order materials, you should ask for impact test, if the material is not impact tested by default.
 