Hello,
I have a PQR done with API 5L Gr. X65 pipe. Can I use this PQR/WPS to weld on an ASME Section VIII, Div. 1 vessel that uses SA-516 70 plate? The P numbers and group numbers are the same for both materials.

Thanks!
 
Were the requirements of ASME Section IX satisfied when the procedure was qualified?
 
PQR was done strictly to ASME IX, satisfying all requirements.
 