Aug 15, 2018 #1 YMech Mechanical Joined Aug 29, 2017 Messages 22 Location US Hello, I have a PQR done with API 5L Gr. X65 pipe. Can I use this PQR/WPS to weld on an ASME Section VIII, Div. 1 vessel that uses SA-516 70 plate? The P numbers and group numbers are the same for both materials. Thanks!
Hello, I have a PQR done with API 5L Gr. X65 pipe. Can I use this PQR/WPS to weld on an ASME Section VIII, Div. 1 vessel that uses SA-516 70 plate? The P numbers and group numbers are the same for both materials. Thanks!
Aug 15, 2018 #2 Don56 Mechanical Joined Feb 18, 2015 Messages 203 Location US Were the requirements of ASME Section IX satisfied when the procedure was qualified? Upvote 0 Downvote
Aug 15, 2018 Thread starter #3 YMech Mechanical Joined Aug 29, 2017 Messages 22 Location US PQR was done strictly to ASME IX, satisfying all requirements. Upvote 0 Downvote
Aug 15, 2018 #4 Don56 Mechanical Joined Feb 18, 2015 Messages 203 Location US Why not then? Upvote 0 Downvote