If I have a GTAW PQR for material P43 to P43 and a GTAW PQR for P1 to P1, can this qualify a PQR for P43 to P1?
 
Replies continue below

Recommended for you

No. Review ASME Section IX, QW-256, under Base Metals, QW-403.11.
 