Good morning all, I have had a question brought to me about the PQR and the welder that performed the test.
Is it mandatory to write a WPQ for the welder that qualified the PQR?

My initial thought was that all welders must have a WPQ written for there qualification.
But if the welder qualified the PQR, would that not be acceptable? Searched Section 9 and ASME interpretations and could not find anything allowing it. Which is probably my answer but wanted to bounce it off of you all.

Thanks
Jmann
 
Replies continue below

Recommended for you

The welder must have a performance qualification record generated even with qualification of a WPS. The PQR can be done concurrent with the WPQR.
 
Jmann,

please see QW-301.2
"......
The welder or welding operator who prepares the WPS qualification test coupons meeting the requirements of QW-200 is also qualified within the limits of the performance qualifications, listed in QW-304 for welders and in QW-305 for welding operators. He is qualified only within the limits for positions specified in QW-303."

That means you must issue a WPQ based on the Procedure Test coupon with the qualification ranges of QW-304 or QW-305 as applicable.

Regards - Juergen
 