Its a pharmaceutical company, dry bulk solid handling, so I can not use water, I just want a relatively basic tool to predict if a mixture will have the potential to segregate or not. I don't (at this stage) need to design a process that will combat the problem, just want to know in general gravitational discharge out of a hopper, (small hopper bins are ussually about 1 meter wide, conical shaped, about 1 meter tall, bottom opening approx 20cm)
any suggestions