Powder Topcoat Mil-Spec...

Status
Not open for further replies.

nicksushi

Industrial
Sep 2, 2003
1
I am looking for the MIL-Spec for Powder Topcoat TGIC Polyester Application. Does one exist?

I have TT-C-490E for the Pre-treatment, however none of my resources have located a spec for powder coat.

Thanks
~nicksushi
 
Replies continue below

Recommended for you

Try MIL-PRF-24712A. The QPL was cancelled, so I don't know if any products qualify to the MIL-SPEC
 