Powder Injection Moulding - literature

Status
Not open for further replies.

bipp

Materials
Jun 15, 2005
3
Dear all,

Does anyone know where I can find reliable literature about the powder injection moulding (PIM) process applied to ceramics?

I need to know the phenomena involved as well as the dependance of the process variables (flow, temperature, viscosity of the binding materials, etc...)

Some links would also be appreciated.

Thanks in advance.
Bipp
 
Replies continue below

Recommended for you

Try this book
R. M. German, Powder Injection Molding, Metal Powder Industries Federation, Princeton, NJ,
1990, 522 pages


 
Basf Germany has probably the largest offering of ceramic feedstocks.
 