WillPowerAutomation
Mechanical
- Feb 18, 2016
- 2
Hello all, a question, I am building a 150 Ton press, it is going to be a 4 post design, I had selected 1084 3" Round Bar for the posts. My machinist wants to use 4140 or 4340 instead of 1084. The posts will be in tension to 150 Tons over a span of 44" threaded on both ends with 2 3/4" UNF thread and nuts. There is no shock loading, force is applied using an air over fluid pump.
Any thoughts or suggestions?
Thanks
WillPower Automation.