we need to install (asap!) a tee connection. however, the tee welds will require pwht but we don't have the time as the plant shutdown cannot be extended.
what we did is that we tapered the ends of the tee connection (three ends) to a thickness where pwht will not be needed and proceeded with the weld connection.
is the tapering of the thickness to forego the pwht allowed? is there a code or a standard that says so? is this good engineering practice? what might be the consequences of our action?
our design pressure is 6.6 mpag while design temperature is 282degC. the tee size is 30-inch diameter with a wall thickness of 25.4mm.
thank you.
what we did is that we tapered the ends of the tee connection (three ends) to a thickness where pwht will not be needed and proceeded with the weld connection.
is the tapering of the thickness to forego the pwht allowed? is there a code or a standard that says so? is this good engineering practice? what might be the consequences of our action?
our design pressure is 6.6 mpag while design temperature is 282degC. the tee size is 30-inch diameter with a wall thickness of 25.4mm.
thank you.