BFZHA
Mechanical
- Oct 29, 2009
- 33
Hi;
Actualy we are working on a WPS for an isolating joint wich have a material with P Number P1 and thickness up to 31.75 mm. Due to welding temperature (250°C)we did not specify a Post Weld Heat Treatement.
We want to know if PWHT requirement is indicated in ASME IX or another standard.
Regards.
Actualy we are working on a WPS for an isolating joint wich have a material with P Number P1 and thickness up to 31.75 mm. Due to welding temperature (250°C)we did not specify a Post Weld Heat Treatement.
We want to know if PWHT requirement is indicated in ASME IX or another standard.
Regards.