We have a situation where the contractor has screwed up during the stressing operation and instead of stressing the 1/2" diameter 270 ksi ultimate strands to 0.8 of fpu (216 ksi or 33kips) they have stressed many of the tendons beyond theoretical yield of 0.9fpu and in one or two cases beyond fpu (without the tendon breaking). The contractor wants to leave the overstressed tendons alone. The only thing we have found on the subject is from page 27 of the document below (State of CA Prestress Manual) related to bridges.
Anyone have advise or suggestions?