Hello everyone,
I bought a stand mixer one year ago and put it in my kitchen countertop. So, this happened on the coating or casing. there are dark brown color spots all around the casing of mixer. Even, one of them bleed near to the power control switch (photo 2). The body is made of die cast aluminum. I suppose it's pitting corrosion but i am not sure. It seems that there's a transparent thin top layer and these spots are formed up under this layer. it's not possible to wipe out these small spots and bleed spot. Anyway, i didn't try with strong chemicals yet. Just used it for 4 or 5 times and cleaned with damp cloth and then with dry one. There is definitely no moisture where the mixer is standing.
do you have any idea what's going on with this coating or body material ? Again i have checked the mechanism of pitting corrosion but couldn't be sure. It might be related to the coating as well.
P.S. i do apologies if this subject is out of forum rules and please let me know if so.
Photo 1
Photo 2
Photo 3
I bought a stand mixer one year ago and put it in my kitchen countertop. So, this happened on the coating or casing. there are dark brown color spots all around the casing of mixer. Even, one of them bleed near to the power control switch (photo 2). The body is made of die cast aluminum. I suppose it's pitting corrosion but i am not sure. It seems that there's a transparent thin top layer and these spots are formed up under this layer. it's not possible to wipe out these small spots and bleed spot. Anyway, i didn't try with strong chemicals yet. Just used it for 4 or 5 times and cleaned with damp cloth and then with dry one. There is definitely no moisture where the mixer is standing.
do you have any idea what's going on with this coating or body material ? Again i have checked the mechanism of pitting corrosion but couldn't be sure. It might be related to the coating as well.
P.S. i do apologies if this subject is out of forum rules and please let me know if so.
Photo 1

Photo 2

Photo 3