Is there a source for porous or microporous high-strength WC or similar materials in rod form for machining?
 
We can supply micro grain. Typically a focus on filtering would describe the pores and a focus on machining would descride the grains. However the language is not all that clear in this area and different people use different terms.

Tom
800 346-8274
Tacoma WA USA
 
microporous high-strength WC ,
how about the pore size? less than 500nm?

It is very difficult to sinter WC with high density and small grain size.
 