Polyurethane vs FRP 2

Status
Not open for further replies.

Joss10

Mechanical
Dec 27, 2012
108
Dear mates,
My contractor is offering me Polyurethane instead of FRP to coat a Crude Oil TK bottom, cost is half.
Any input will be apreciated.
 
Replies continue below

Recommended for you

What advantages (besides price) is he touting?
IF you need strength then FRP has big advantages.
Either way the adhesion is the primary issue, make sure that you know what combination of surface prep and base coats are being used to assure proper adhesion.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
The coatings aren't even close to being equivalent. Which one do you need? I have no idea, but I'm pretty sure there is some API and/or NACE guidance available on the topic if you do some research.
 
Dear Joss10,

FRP is indeed a heavy duty coating. High build PU is very much abrasion resistant too.

So I would suggest if your Crude oil property is good for PU, then go for it!!

CocoE
 
I would not use a polyurethane in this situation. I would recommend a Cyclo-Aliphatic Epoxy. They're designed for immersion in these situations. Polyurethanes are generally used for UV protection, gloss retention, etc.
 