Team I had a molded very thin wall polyurethane rubber

After the molding the parts are so sticky that I put them into a chlorine bath

The problem is that after the wash the parts suffer from discoloration

There is any alternative lubricant/coating to decrease this tackiness and stiffness ?

Taking into account that this is a medical application.

Regards
 
Replies continue below

Recommended for you

It sounds as if the urethane was not fully mixed, not mixed in the right ratio, or not subjected to a long enough cure at a high enough temperature...i.e. you have un-cured parts.

Did you perhaps not put in a full amount of "hardener" expecting to get a finished product with a lower durometer (lower stiffness)? That don't work. Get a compound that is formulated to cure at a lower durometer, and mix at the recommended ratios.
 