Jun 7, 2010 #1 jmonti Civil/Environmental Joined Jun 7, 2010 Messages 3 Location US Hi Would anyone know if polyurethane foam is considerd a "combustible fiber" and would need to classified as a H 3 use
Hi Would anyone know if polyurethane foam is considerd a "combustible fiber" and would need to classified as a H 3 use
Jun 7, 2010 1 #2 pipesnpumps Mechanical Joined Dec 4, 2002 Messages 316 Location US It is a group A plastic (NFPA 13 5.6.4.1). I would personally say it is NOT a combustible fiber per IBC definition (307.2). Upvote 0 Downvote
It is a group A plastic (NFPA 13 5.6.4.1). I would personally say it is NOT a combustible fiber per IBC definition (307.2).