I cannot seem to find fluid properties (density, spec heat, therm cond, or viscosity) for a 50/50 mixture of polypropylene glycol/water mixture.

I am going to need the fluid properties for this mixture across a range of temps, (100-300F).

If anyone knows a good source where i might find this data i would realy appriciate it.

Thank you
 
short of getting the information from the mfg, the ASHRAE Handbook has propylene glycol/water and ethylene glycol/water properties listed in tables for use. the properties listed in the handbook are density ,viscosity, specific heat capacity, thermal conductivity, etc. from what i remember. your local library may have this handbook or even a good bookstore.

good luck!
-pmover
 