Please recommend me some polymeric products that have these properties:
1.High dielectric constant
2.Adhesive
3.Biocompatible
4.Clear
5.In spray format

number 4 and 5 are not necessary but I prefer it that way.
Please do not forget the links
Thank you
 
Replies continue below

Recommended for you

Water has a particularly high dielectric constant so water based adhesive that retains some water might meet your needs. These include gelatin, starch, and silicates.
 
How high is high? For moderate values like 6, you could use polyurethane or Kynar, both are flexible and can have adhesive applied to them, but polyurethane can be foamed on.

TTFN
I can do absolutely anything. I'm an expert!