Hi,
I am looking for material(Polymer) which has high coefficient of friction and high hardness value.Please tell me if you know one.
Our problem is we are currently using Nylon as clamping jaw plate surface material. (For clamping steel wires) But there is a slippage problem from the clamps. So I was looking for a polymer with high coefficient of friction(Lowering Slippage) and high hardness (Hardness lower than steel.
 
Replies continue below

Recommended for you

You need a filled polymer. Add some wollastonite or glass fiber to your polymer. They should increase COF and hardness.

Look for materials for free at or contact a company with plenty of material options such as RTP or PolyOne.

Chris DeArmitt

"Knowledge has no value except that which can be gained from its application toward some worthwhile end."
Think and Grow Rich - Napoleon Hill
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor