PolyMaker

Automotive
Jun 2, 2010
2
Are there any potential "itch" or squeek issues with using a 20% GF Nylon substrate with a soft PVC overmold?

How about a 20% GFNylon against an Olefin?

Any feedback or direction to additional resoures would be appreciated.

Best Regards,
RonB
 
Replies continue below

Recommended for you

I don't know but if you do have problems you should be able to fix them with additives that alter friction. Squeak is due to stick-slip sliding of one material on the other.

Chris DeArmitt PhD FRSC CChem

Consultant to the plastics industry
 
Thanks Chris - good to know we can likely handle it w/ additives if need be. Any suggestions on where I might find a cBSR ompatability matrix of some sort?
 
Hi PolyMaker,

What you ask is an interesting question. I don't know of one. As the effect relies on surface friction, it would be very sensitive to additives including antioxidants, UV stabilizers, slip aids, anti-blocks etc.. That means that you can't predict what a polymer pair will do because it's more about the additives than the polymers themselves.

When I worked at BASF they claimed that their ABS/PA blend never squeaked and that was a selling point (commercial name Terblend N). I always wondered why that would be.

Chris DeArmitt PhD FRSC CChem

Consultant to the plastics industry
 
Chris

It can be important on interior trim and dashboard components on cars.

BASFs opposition unkindly refereed to that range as Terdblend



Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
Oh, I understand why no squeak is important but not why an ABS nylon blend would have that property.

Mechanically, it's a lot like ABS/PC.

Chris DeArmitt PhD FRSC CChem

Consultant to the plastics industry
 