MadMango
Mechanical
- May 1, 2001
- 6,992
I need to spec a UL-94 V-0 material for an injection molded trim ring, approximately 5.5" OD U-shaped. The material needs to be translucent (70-80%), but have an option to be metalized or have color added to it. It also needs to be flexible so it can be snapped into position without secondary fasteners. I'm not a materials guy, but my Google searching has led me to polyethersulfone (Veradel A-301). Is there a more common material that I have missed?
"Art without engineering is dreaming; Engineering without art is calculating."
Have you read faq731-376 to make the best use of these Forums?
"Art without engineering is dreaming; Engineering without art is calculating."
Have you read faq731-376 to make the best use of these Forums?