Looking for applications of Poly 4 Methyl Pentene 1 (also named PMP, TPX) in the automotive industry.
Where is it currently being used, what are the potential future applications?
Could a significant price range open new applications for this product?
Who are currently the main suppliers ?

Regards,
Laurence
 
Replies continue below

Recommended for you

Anywhere where transparent grades of PP are being considered, but won't stand the temperature.

Anywhere where polycarbonate is being considered, but fails due to chemical resistance

Regards
pat
 