Hi,
I want to know if there is any way to polish stainless steel through chemicals. Currently, I am doing electropolishing process on parts but I need something simpler process.

Thanks
 
If you use the same chemicals but hotter and more concentrated you get a little bit of the effect.
Simpler? Automate your EP system.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 