Mar 14, 2003 #1 chen2003 Materials Joined Mar 14, 2003 Messages 2 Location AT Hi, I want to check the Poisson's ratio of 42CrMoS4. But I can not find it. Who can tell me where I can get it? Thank you in advance. Best regards chen2003
Hi, I want to check the Poisson's ratio of 42CrMoS4. But I can not find it. Who can tell me where I can get it? Thank you in advance. Best regards chen2003
Mar 17, 2003 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US Poisson's ratio is generally accepted to be 0.29 for steel. Upvote 0 Downvote