Poisson ratio

Status
Not open for further replies.

blckwtr

Mechanical
Oct 30, 2006
204
Hi, all. Is it possible to derive poisson ratio purely from uniaxial stress strain response?
 
Replies continue below

Recommended for you

I'm quite positive you cannot do this, since the poissons ratio is by definition the ratio between the tranvserse train to the axial strain. You need both values in order to be able to calculate the ratio.
 