Dec 12, 2019 #1 Resegone Mechanical Joined Nov 9, 2019 Messages 19 Location IT Hi everyone i ask an info about PMRC MAR GS/105 or GS/106. What is it? My customer ask to provide this standard for grahpite packing. But i don't know what is it and i didn't find anything! Maybe is refer to Philippine Mineral Reporting Code? Thx everyone.
Hi everyone i ask an info about PMRC MAR GS/105 or GS/106. What is it? My customer ask to provide this standard for grahpite packing. But i don't know what is it and i didn't find anything! Maybe is refer to Philippine Mineral Reporting Code? Thx everyone.
Apr 13, 2020 #2 JChanMe Industrial Joined Aug 19, 2009 Messages 11 Location US PMRC MAR GS/105 and GS/106 are PETRONAS technical standards, which are additional requirements to ASTM F2168 and F2191 for graphite packing materials. James Chan Upvote 0 Downvote
PMRC MAR GS/105 and GS/106 are PETRONAS technical standards, which are additional requirements to ASTM F2168 and F2191 for graphite packing materials. James Chan