We're considering investing in a PMI instrument. Does anyone have any experience with Spectro PMI instruments? The model I'm looking at is a TXC01.
thanks,
 
Replies continue below

Recommended for you

The choice of equipment depends on intended application. In case analysis of Carbon and Phosphorus is not an issue, you must seriously consider equipment working on X-Ray Flourescence. During the last five years, these equipments have gone a sea change. You no longer require Isotopes.

The advantages of X-ray flourescent equipment are many. Most striking advantages are:
-Lightweight of gun and usability under all conditions
-Does not generate an arc or a spark, which means that you could use it in an operating refinery, etc.

 
I have had very good experience with the Spectrosort and Spectroport PMI equipment for field PMI work. They are especially useful when light elements are required to be examined; e.g.,aluminum alloys.

We, like rkg, have purchased x-ray tube XRF PMI equipment, which more suits our general purpose needs.


 
Thanks, guys.

In our case we want to be able to check for Carbon and other elements.
 