May 9, 2011 #1 Lou47 Structural Joined Dec 6, 2010 Messages 2 Location US Has the PMA 22 sheet piling section become obsolete?
May 9, 2011 #2 BAretired Structural Joined Nov 16, 2008 Messages 10,982 Location CA Not according to Mr. Google. http://www.google.ca/search?hl=&q=P...lient-ff&rlz=1B3GGLL_en-GBCA404CA404&ie=UTF-8 BA Upvote 0 Downvote
Not according to Mr. Google. http://www.google.ca/search?hl=&q=P...lient-ff&rlz=1B3GGLL_en-GBCA404CA404&ie=UTF-8 BA
May 9, 2011 1 #3 SlideRuleEra Structural Joined Jun 2, 2003 Messages 5,527 Location US If you mean "Can PMA 22 sheet pile be ordered from the mill, new?". I believe the answer is "no". PMA 22 was a U.S. Steel designation. That company has changed much over the past few years. I don't see that product on their website: http://www.uss.com/corp/index.asp Another current manufacturer of steel sheet pile is Nucor-Yamato... don't see an equivalent for PMA 22 there either: http://www.nucoryamato.com/staticdata/RollCastSchedule.pdf?currdate=5/9/2011 12:43:24 PM Arcelor Mittal makes products similar to PMA 22, but not the same dimensions. See page 14 of their current catalog: http://www.arcelormittal.com/sheetpiling/uploads/files/AMCRPS_Gen_Cat_EN_2011.pdf http://www.SlideRuleEra.net http://www.VacuumTubeEra.net Upvote 0 Downvote
If you mean "Can PMA 22 sheet pile be ordered from the mill, new?". I believe the answer is "no". PMA 22 was a U.S. Steel designation. That company has changed much over the past few years. I don't see that product on their website: http://www.uss.com/corp/index.asp Another current manufacturer of steel sheet pile is Nucor-Yamato... don't see an equivalent for PMA 22 there either: http://www.nucoryamato.com/staticdata/RollCastSchedule.pdf?currdate=5/9/2011 12:43:24 PM Arcelor Mittal makes products similar to PMA 22, but not the same dimensions. See page 14 of their current catalog: http://www.arcelormittal.com/sheetpiling/uploads/files/AMCRPS_Gen_Cat_EN_2011.pdf http://www.SlideRuleEra.net http://www.VacuumTubeEra.net