Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Plywood Tensile Strength 2

Status
Not open for further replies.

LPPE

Structural
Joined
May 16, 2001
Messages
578
Location
US
Anyone have values for the tensile strength of plywood, or know where to find them? I have the Canadian Plywood Association Plywood Design Fundamentals, and there are some values in N/mm, and when I convert to english units, I come up with some really weak plywood.
 
Go to apawood.org, download "Plywood Design Specification", see Table 3
 
Tension in the Plane of the plies Species Group 4,"Ft" varies from Dry Stress Grades S1=1300psi, S2=1100psi and S3=1100psi also. US Product Standard PS-1-83 is the testing basis. Good Luck.
 
Status