We have a Florida job that needs to be sealed by another engineer.
They have used a formula to calculate the section modulus for plywood.
The formula is:

Save= {(# of plies) Su + (# of plies) Sperp]
--------------------------------------
(Total # of Plies)

Reslutant S = Save ( total # of plies )2

Here is an example using 5/8" plywood:

Save= {(1) 0.361 + (2) 0.238] = 0.279 in3 / ft
-----------------------
(3)

Resultant S = 0.279( 3 )2 = 2.511 in3 / ft

The formula is used to calculate the bending stress fb = M/S

Does anyone know how these formulas were derived? Why is an average calculated then it is multiplied by the total number of plies squared? Is this an engineering mechanics problem?

 
Replies continue below

Recommended for you

Recommend KS be used in bending strength calculations, instead of Section modulus.

See:
Plywood Design Specification Form D510,
 