Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Plywood Section Modulus

Status
Not open for further replies.

jtrenam

Civil/Environmental
Joined
Jul 31, 2008
Messages
1
Location
US
We have a Florida job that needs to be sealed by another engineer.
They have used a formula to calculate the section modulus for plywood.
The formula is:

Save= {(# of plies) Su + (# of plies) Sperp]
--------------------------------------
(Total # of Plies)

Reslutant S = Save ( total # of plies )2

Here is an example using 5/8" plywood:

Save= {(1) 0.361 + (2) 0.238] = 0.279 in3 / ft
-----------------------
(3)

Resultant S = 0.279( 3 )2 = 2.511 in3 / ft

The formula is used to calculate the bending stress fb = M/S

Does anyone know how these formulas were derived? Why is an average calculated then it is multiplied by the total number of plies squared? Is this an engineering mechanics problem?

 
Recommend KS be used in bending strength calculations, instead of Section modulus.