As far as my knowledge goes, this configuration of welding is non-standard as per Sec-IX. It will be difficult to ensure complete fusion and removal of slags. Alternative suggestion is use properly fitting 1/4"x20 plug and seal weld at top.
 
You didn't get an actual answer, to a question that contained no context.
Where is the finished part going to spend the rest of its life?


"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Be very careful about your sketch: The question asks about a 1/4" hole in a 1/5" "pin" - but as-drawn, the pin looks like 3/32 (or smaller!) hole less then 1/4 inch in a relatively long 3 inch tapered dowel. But the dimensions call for a 1/4 inch tapped hole 0.75 inch deep in a 0.50 diameter dowel less than 2.0 inch long top of the dowel!

The recommended seal weld around the 1/4-20 NC tapped hole allows less than a 1/8 inch fillet around the 1/4 inch plug Does the dowel (pin) need to be removed later? What kind of alloy is the pin - this will control what kind of set screw and weld is allowable/needed.
 
Material is A36 and the tapered side of the pin is fillet welded on the distribution gas pipeline to abandon the service (100 psi max) using an in-service welding procedure. The sketch is not to scale. I am not considering plugging 1/4x20 threaded hole on top of the pin an in-service weld.
 