JasonLouie
Materials
Hello,
I have a weld map which shows 1" deep plug welds. The vendor changed the welding symbol from a plug weld to a fillet welds since he claims that the plug weld was done with a fillet weld fill procedure (I don't know what this means).
My questions are: Are plug welds considered to be full penetration welds or fillet welds? If the plug weld is 1" deep, do I need a weld procedure qualified for 1"? If it is a fillet weld, then weld metal and base material thickness are not applicable (as per ASME IX), correct?
The vendor has a weld procedure qualified to maximum 3/4" and is trying to use this procedure for the plug welds. I appreciate any help anyone can provide! Thank you very much.
I have a weld map which shows 1" deep plug welds. The vendor changed the welding symbol from a plug weld to a fillet welds since he claims that the plug weld was done with a fillet weld fill procedure (I don't know what this means).
My questions are: Are plug welds considered to be full penetration welds or fillet welds? If the plug weld is 1" deep, do I need a weld procedure qualified for 1"? If it is a fillet weld, then weld metal and base material thickness are not applicable (as per ASME IX), correct?
The vendor has a weld procedure qualified to maximum 3/4" and is trying to use this procedure for the plug welds. I appreciate any help anyone can provide! Thank you very much.