Does anyone have info on the structural properties of plexi glass?

much apreciated
 
Replies continue below

Recommended for you

You should contact the manufacturer. They would probablly have the best data.

Wes C.
 
Thanks wes616, but I don't know of any manufacturer. The design will be done before a mfr is chosen.

 
I also recommend you contact the manufacturer. If you don't have one chosen, dig in the phone book or the net and call around to a couple. It might be on the net somewhere anyway, have you "Googled" it?
 
I've googled it and managed to get a few results:
bending stress of 11 ksi,and a youngs modulus of 450ksi.

I've also contacted a few manufacturers, but no replies.
 
If you sound interested in a product, any sales rep should jump all over to get you the information you need.

Those values sound good to me...

Generic Values for Acrylic are

Sut = 10Ksi

Suc = 18Ksi



Wes C.
------------------------------