Please explain,
As per ASM sec.VIII Dev.1 if two indication found in RT Film of weld joint what is the acceptance criteria for that
 
Ok sir, Thanks for your information
I have seen in that. If two indications present in weld, the max permissible size is 4mm. It is correct or not.
 