Please could you give me ASTM equivalents of the following materials;

BS EN 10025 S275 (black plate, bar & rolled sections for general fabrication)

BS1501 151/161 Grade 430B (boiler quality plate)

BS 970 080M40 (shafts)

BS 970 080M40 Normalised after forging (shafts)

Bright mild steel bar - BS970 070M20 (for machined components)

Cast iron: BS1452 Grade 300 (bearing housings)

Heat-resisting cast iron: Meehanite type HS C: 2.9 - 3.1%, Si: 4.75 - 5.25%, S: 0.010% max, P: 0.100% max, Mn: 0.6 - 0.8%, Cr: up to 0.5% (cast door and door frame)

Lead bronze: BS EN 1982:1998 Table 30-CuSn5Pb20-C (castings - bearing bushes and thrust washers)

Stainless steel grade 304 (plate - kiln feed chute)

Stainless Steel to BS1449 Part 4 1967 Grade 310 S24 (plate)

High alloy cast steel to BS3100:1991 Grade 310 C40, with max working temp of 1200°C (stainless steel casting - nose ring for kiln cooling air shell)

Stainless steel grade 316L (plate - kiln discharge hood)

Hexagon head bolts, screws and nuts to BS 4190 grades 4.6 / 4 (Metric)

Hexagon head bolts, screws and nuts to BS 3692 grades 8.8 / 8 (Metric)
 
outspan,

You may want to see TVP's post in thread330-89970 for links to resources that can help you do this.



Best regards,

Matthew Ian Loew
"I don't grow up. In me is the small child of my early days" -- M.C. Escher

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
BS EN 10025 S 275 , Refer A 36

BS 1510 Refer A 20 , A 516, A 515

For Steel Grade S 304, 316, 310, There are so many STD for different Product forms. A 182 for Forging, A 312 for Pipes, A 213 for tube, A 269 for Tube, A 240 for Plates. and so on
 