Sep 19, 2002 #1 rubepierre Industrial Joined Dec 15, 2001 Messages 30 Location US is this recomended- -or can it be done within normal operating procedures- -I myself have doubts- -comments??
is this recomended- -or can it be done within normal operating procedures- -I myself have doubts- -comments??
Sep 19, 2002 #2 pipewelder1999 Industrial Joined Mar 17, 2002 Messages 309 Location US I'm not an expert on plating but based on what I know about the process and JB weld. No it cannot be done. Hopefully someone will correct me if I'm wrong. Gerald Austin Iuka, Mississippi http://www.weldinginspectionsvcs.com Upvote 0 Downvote
I'm not an expert on plating but based on what I know about the process and JB weld. No it cannot be done. Hopefully someone will correct me if I'm wrong. Gerald Austin Iuka, Mississippi http://www.weldinginspectionsvcs.com
Sep 19, 2002 #3 GRoberts Materials Joined Apr 22, 2002 Messages 548 Location US I don't know about normal plating, but vapor deposition and thermal spray could be done. Upvote 0 Downvote